Research Article
Residual Stress Distribution in Selective Laser Melting of SS316L Parts
Table 1
SLM process parameters used to build samples.
| S. no. | Build parameter (units) | Value |
| 1 | Laser power (W) | 130 W | 2 | Laser beam diameter | 55 μm | 3 | Scanning speed | 500 mm/sec | 4 | Powder grain size | 20 to 40 μm | 5 | Layer thickness | 40 μm | 6 | Process time per specimen | 3 h | 7 | Hatch distance | 80 μm |
|
|