Contribution rates of different phases to the mechanical properties of CCAM.

Mixture typeContribution rate to Cantabro loss/(%)
Interface (without balls)PAM (without balls)Cement (without balls)

BAM3.27096.73
SAM5.36094.64
HAM1.317.1781.52

Interface (with balls)PAM (with balls)Cementitious network (with balls)

BAM34.02065.98
SAM35.44064.55
HAM27.2117.1755.61

Mixture typeContribution rate to IDT strength @ 15°C/(%)
Interface (without balls)PAM (without balls)Cement (without balls)

BAM−0.5928.8271.76
SAM−6.9629.7577.22
HAM−38.3546.6291.73

Interface (with balls)PAM (with balls)Cementitious network (with balls)

BAM58.2328.8212.94
SAM56.3329.7513.92
HAM36.8446.6216.54

Mixture typeContribution rate to IDT strength @ −10°C/(%)
Interface (without balls)PAM (without balls)Cement (without balls)

BAM22.8731.9145.21
SAM12.3641.9345.69
HAM6.5442.8550.59

Interface (with balls)PAM (with balls)Cementitious network (with balls)

BAM58.5131.919.57
SAM48.3941.939.68
HAM46.4342.8510.71

Mixture typeContribution rate to SCB peak force @ 25°C/(%)
Interface (without balls)PAM (without balls)Cement (without balls)

BAM50.4917.4532.06
SAM28.9627.6943.35
HAM29.4929.6240.89

Interface (with balls)PAM (with balls)Cementitious network (with balls)

BAM72.9317.459.62
SAM59.2927.6913.01
HAM58.1129.6212.27

Mixture typeContribution rate to SCB peak force @ −10°C/(%)
Interface (without balls)PAM (without balls)Cement (without balls)

BAM−9.8937.3172.58
SAM−12.34666.3
HAM−28.7559.8168.93

Interface (with balls)PAM (with balls)Cementitious network (with balls)

BAM44.0837.3118.61
SAM37.04616.99
HAM22.5259.8117.67