ANOVA analysis for the S/N ratio of microhardness.
| ANOVA response table for the S/N ratio | Source | DF | Seq SS | Adj SS | Adj MS | F values | values | Sintering temperature (°C) | 2 | 1.70683 | 1.70683 | 0.853411 | 236.61 | 0.005 | Sintering pressure (MPa) | 2 | 0.30054 | 0.30054 | 0.150267 | 41.667 | 0.024 | Sintering time (min) | 2 | 0.46283 | 0.46283 | 0.231413 | 64.17 | 0.016 | Error | 2 | 0.00722 | 0.00722 | 0.003608 | | | Total | 8 | 2.47740 | | | | |
| Ranking response table for the S/N ratio | Level | Sintering temperature (°C) | Sintering pressure (MPa) | Sintering time (min) | 1 | 33.91 | 34.24 | 34.56 | 2 | 34.86 | 34.02 | 34.04 | 3 | 33.97 | 34.47 | 34.13 | Delta | 0.96 | 0.46 | 0.53 | Rank | 1 | 3 | 2 |
|
|