Investigating the Microstructure, Tensile Strength, and Acidic Corrosion Behaviour of Liquid Metal Stir Casted Aluminium-Silicon Carbide Composite
Table 2
Acidic immersion corrosion experiment results.
| Run | Acidic solution | Immersion time | Wt. % of reinforcement | Corrosion rate mm/yr |
| 1 | HCl | 30 | 0 | 11.66 | 2 | HCl | 56 | 10 | 12.13 | 3 | HCl | 80 | 20 | 14.01 | 4 | HNO3 | 30 | 10 | 9.91 | 5 | HNO3 | 56 | 20 | 11.24 | 6 | HNO3 | 80 | 0 | 7.15 | 7 | H2SO4 | 30 | 20 | 11.46 | 8 | H2SO4 | 56 | 0 | 4.83 | 9 | H2SO4 | 80 | 10 | 12.34 |
|
|