Research Article

Dry Sliding Wear Behavior of Copper Matrix Composites Enhanced with TiO2 and MoS2 Hybrids

Table 3

Analysis of variance for the wear rate.

ParametersDFSeq SSAdj SSAdj MSF%

Molybdenum percentage20.00000070.00000070.00000033.440.22511.48
Load (N)20.00000020.00000020.00000010.990.5013.28
Sliding velocity (m/s)20.00000510.00000510.000002526.440.03683.61
Total80.0000061

S = 0.000310028, R-Sq = 96.86%, R-Sq (adj) = 87.45%.