Research Article

Preparation and Characterization of Hydroxyapatite Coating on AZ31 Mg Alloy for Implant Applications

Figure 5

SEM images of coating obtained at −1.4 V before and after immersion in SBF solution for 1 day and 7 days.
175756.fig.005a
(a)
175756.fig.005b
(b)
175756.fig.005c
(c)