Research Article
Effect of Surface Treatment with Alkaline Agents at Two Different Temperatures on Microshear Bond Strength of Zirconia to Composite Resin
Table 3
Pairwise comparisons of the groups regarding μSBS.
| Group (I) | Group (J) | Mean difference | value |
| Control | NaOH | -5.75 | <0.001 | NaOH+ heat | -6.30 | <0.001 | Zr(OH)4 | -10.03 | <0.001 | Zr(OH)+ heat | -10.35 | <0.001 |
| NaOH | Control | 5.75 | <0.001 | NaOH+ heat | -.0.54 | 0.854 | Zr(OH)4 | -4.27 | <0.001 | Zr(OH)+ heat | -4.60 | <0.001 |
| NaOH+ heat | Control | 6.30 | <0.001 | NaOH | 0.54 | 0.854 | Zr(OH)4 | -3.73 | <0.001 | Zr(OH)4+ heat | -4.05 | <0.001 |
| Zr(OH)4 | Control | 10.03 | <0.001 | NaOH | 4.27 | <0.001 | NaOH+ heat | 3.73 | <0.001 | Zr(OH)4+ heat | -.0.32 | 0.975 |
| Zr(OH)+ heat | Control | 10.35 | <0.001 | NaOH | 4.60 | <0.001 | NaOH+ heat | 4.05 | <0.001 | Zr(OH)4 | 0.32 | 0.975 |
|
|