Improving the Performance of Reprocessed ABS Products from the Manufacturing Perspective via the Taguchi Method
Table 9
Comparison of product performance for virgin ABS and R-40 before and after optimization.
| Criteria | Hoop tensile strength (MPa) | Elongation at break (%) | Shrinkage (%) |
| Virgin ABS | 50.22 | 3.81 | 0.0985 | R-40 before optimization | 49.28 | 3.74 | 0.1123 | R-40 after optimization | 50.74 | 4.89 | 0.0075 |
|
|