[Retracted] Comparison of Microstructure and Mechanical Properties of A356/SiC Metal Matrix Composites Produced by Two Different Melting Routes
Table 8
Improved tensile strength of A356/SiC MMC by electromagnetic stir casting process.
|
A356/SiC MMC |
Sample number | Electromagnetic stir casting samples (ESCS) | Mechanical stir casting samples (MSCS) |
Improved tensile strength (MPa) | Tensile strength (MPa) | Variation (MPa) | Average tensile strength (MPa) | Tensile strength (MPa) | Variation (MPa) | Average tensile strength (MPa) |
| 100% A356 + 0% SiC | 1 | 232 |
4 |
232.66 | 235 |
7 |
231.33 |
0.57% | 2 | 235 | 231 | 3 | 231 | 228 |
| 95% A356 + 5% SiC | 1 | 274.6 |
4.7 |
274.23 | 268.5 |
14.1 |
266.96 |
2.65% | 2 | 271.7 | 278 | 3 | 276.4 | 254.4 |
| 90% A356 + 10% SiC | 1 | 292 |
2.5 |
290.63 | 258.8 |
36.2 |
280.13 |
3.61% | 2 | 289.5 | 286.6 | 3 | 290.4 | 295 |
| 85% A356 + 15% SiC | 1 | 310 |
7.5 |
309.83 | 318.6 |
46.6 |
298.2 |
3.75% | 2 | 313.5 | 304 | 3 | 306 | 272 |
|
|