Research Article
Effect of Curing on the Tensile and Flexural Performance of Fully Biodegradable Corn Starch/Areca Frond Composites
Table 6
Flexural properties of composites.
| Curing environment | Maximum load (N) | Maximum flexural extension (mm) | Average flexural stress (MPa) |
| Sunlight | 34.79 | 14.24 | 16.06 | OTG oven | 48.07 | 6.34 | 22.19 | Steam oven | 73.99 | 8.29 | 34.15 | Hot air oven | 60.82 | 12.10 | 28.07 |
|
|