Figure 4
Decomposed relaxation process of NBR for seven representative temperatures (a) 404 K (b) 359 K (c) 326 K (d) 293 K (e) 272 K (f) 251 K, and (g) 233 K. Five relaxation processes, α′ (black dashed line), α (red dashed line), β (blue dashed line), γ (gray dashed line), and conduction (navy dashed line), contribute to the imaginary permittivity data.
(a) |
(b) |
(c) |
(d) |
(e) |
(f) |
(g) |