Research Article

Structural Properties of Liquid SiC during Rapid Solidification

Figure 4

The ADF of SiC at 4500 K and 100 K. ((a), (c) at 4500 K and 100 K, Si as central atom, CN-3, 4, 5, 6; (b), (d) at 4500 K and  100 K, C as central atom, CN-2, 3, 4).
273023.fig.004a
(a)
273023.fig.004b
(b)
273023.fig.004c
(c)
273023.fig.004d
(d)