Research Article

Strength and Durability Performance of Alkali-Activated Rice Husk Ash Geopolymer Mortar

Table 1

Composition of alkali activators used for the investigation.

KeyMass ratio of solution (1 : 2.5)Composition of GP liquor
Na-silicate NaOH TotalNa2OSiO2H2OTotal

7 M3.101.244.340.681.342.324.34
8 M3.181.274.450.721.382.354.45
9 M3.231.294.520.761.402.364.52
10 M3.301.324.620.811.432.384.62